Resources / Blog
Blog
Engineering notes, process explainers and production insights from the VONTOC team.

Shrinkage Injection Molding: Chart, Formula & Fixes
Accurately predict shrinkage by applying the formula $S = (D_m - D_p) / D_m \times 100\%$, accounting for material-specific rates…
Read more
Injection Molding Surface Finish: SPI vs VDI Guide
SPI standards define polished finishes from A1 to D3, while VDI 3400 specifies EDM textures ranging from 12 to 45.…
Read more
Clear Cast Acrylic Sheets: Buy & Specs
Select clear cast acrylic sheets with a light transmission rate exceeding 92% and a thickness tolerance of ±0.1 mm for…
Read more
ABS Injection Molding: Guide, Settings & Fixes
Optimize ABS injection molding by maintaining melt temperatures between 210°C and 250°C with mold cooling at 40°C to 80°C. Prevent…
Read more
PC Injection Molding: Params, Design & Tips
Polycarbonate requires 280–320°C melt temperatures and thorough drying to <0.02% moisture to prevent hydrolysis. Design uniform wall thicknesses between 2.0–3.5…
Read more
TPE Injection Molding: Guide, Settings & Tips
Successful TPE injection molding requires precise control of melt temperature between 180°C and 230°C to prevent degradation while ensuring flow.…
Read more
Can Mold Release Agent Cause Overmold Delamination?
Yes. Mold release agent can interfere with adhesion between an overmold and its substrate and, in some cases, contribute to…
Read more
TPU Injection Molding: Guide, Design & Tips
TPU injection molding requires precise control of melt temperature between 190°C and 230°C to prevent degradation while ensuring flow. Design…
Read more
PMMA Injection Molding: Process, Defects & Tips
PMMA injection molding demands precise melt temperatures of 230–260°C and high injection pressures to prevent flow marks and internal stress.…
Read more